Stress distribution of tempered sight glass
Click:
-Time:1970-01-01 08:00
Stress distribution of tempered sight glass
Explanation of super end stress distribution of B. tempered sight glass
The final stress distribution map of toughened sight glass shows larger compressive stress on the outer surface, decreasing from the outer layer to the center, and increasing tensile stress in the center layer. Tensile stress decreases from center to outer layer, and tensile stress and compressive stress at e point are 0.
A. began to heat the tensile stress stress pressure stress 0 temperature a outer layer: high temperature inner layer: low temperature outer layer: compressive stress inner layer: tensile stress.
B. continued to heat the tensile stress stress stress 0 temperature C, B temperature difference in inner and outer layer gradually reduced, and the stress value also decreased to no.
C. began to cold (2 seconds) Zhang Yingli pressure stress 0 temperature c c outer layer fast cold, low temperature, the inner layer is still in high temperature, the outer layer of Zhang Yingli.
D. suddenly quenched (within 5 seconds), Zhang Yingli compressive stress 0 temperature and temperature D, the temperature of inner and outer layer decreased, the temperature difference decreased, the inner layer began to shrink, the outer surface was below 500 degrees, and the outer layer had compressive stress.
E. continues to cold (in 12 seconds) Zhang Yingli compressive stress 0 temperature c e inner layer also down to about 500 degrees C, the internal and external stress basically formed.
F. toughening is completed (20 seconds), tensile stress, compressive stress 0 temperature, 20 degrees C, 650 C, 470 C - 500 C F, the temperature inside and outside is decreased, the trend of temperature difference is balanced, and the long-term stress inside and outside is formed.

If you are interested in the tempered sight glass or need to consult, please click on our online customer service, or call us. Pan Chao, customized different quality specifications of the glass.
Pan Chao special industrial glass, tailored for your different quality of the glass.
Welcome sending your inquiry: Phone : +86 13569413718 Email: info@panchaoglass.com
Explanation of super end stress distribution of B. tempered sight glass
The final stress distribution map of toughened sight glass shows larger compressive stress on the outer surface, decreasing from the outer layer to the center, and increasing tensile stress in the center layer. Tensile stress decreases from center to outer layer, and tensile stress and compressive stress at e point are 0.
A. began to heat the tensile stress stress pressure stress 0 temperature a outer layer: high temperature inner layer: low temperature outer layer: compressive stress inner layer: tensile stress.
B. continued to heat the tensile stress stress stress 0 temperature C, B temperature difference in inner and outer layer gradually reduced, and the stress value also decreased to no.
C. began to cold (2 seconds) Zhang Yingli pressure stress 0 temperature c c outer layer fast cold, low temperature, the inner layer is still in high temperature, the outer layer of Zhang Yingli.
D. suddenly quenched (within 5 seconds), Zhang Yingli compressive stress 0 temperature and temperature D, the temperature of inner and outer layer decreased, the temperature difference decreased, the inner layer began to shrink, the outer surface was below 500 degrees, and the outer layer had compressive stress.
E. continues to cold (in 12 seconds) Zhang Yingli compressive stress 0 temperature c e inner layer also down to about 500 degrees C, the internal and external stress basically formed.
F. toughening is completed (20 seconds), tensile stress, compressive stress 0 temperature, 20 degrees C, 650 C, 470 C - 500 C F, the temperature inside and outside is decreased, the trend of temperature difference is balanced, and the long-term stress inside and outside is formed.

If you are interested in the tempered sight glass or need to consult, please click on our online customer service, or call us. Pan Chao, customized different quality specifications of the glass.
Pan Chao special industrial glass, tailored for your different quality of the glass.
Welcome sending your inquiry: Phone : +86 13569413718 Email: info@panchaoglass.com
Related articles
- How to Evaluate the Service Life of Tempered Sight Glass
- Is the Safety of Tempered Glass Overestimated?
- Why Tempered Glass Is Not Suitable for On-Site Size Modificat
- Classification of tempered glass
Recommend
- What Happens When Glass Materials Have Mismatched Thermal Exp
- How to Evaluate the Service Life of Tempered Sight Glass
- Why Glass Tube Length Tolerance Matters More Than You Think
- How Glass Material Affects Optical Testing Results
- Core Differences Between Industrial Glass and Laboratory Glas
- How Glass Tube Ovality Affects Sealing Performance
- Why Does Sight Glass Require Independent Pressure Testing?
- How Different Annealing Processes Affect Glass Performance
- Is the Safety Valve of a Liquid Nitrogen Tank Really “Just
- Is the Safety of Tempered Glass Overestimated?
Rank
- Application of high temperature resistant glass
- Precautions in the process of quartz tube cutting and picklin
- Chemical Stability Testing Standards for Borosilicate Glass
- Anti-Fog Treatment Techniques for Sight Glass: A Technical Ov
- The Impact of Thermal Expansion Coefficient on Glass Material
- The difference between high borosilicate glass, medium borosi
- Introduction to Borosilicate Glass
- High Temperature Resistant Glass: protecting world under extr
- What Glass Has the Highest Temperature Resistance
- What are the advantages and disadvantages of quartz tube heat
Latest articles
- What Happens When Glass Materials Have Mismatched Thermal Exp
- How to Evaluate the Service Life of Tempered Sight Glass
- Why Glass Tube Length Tolerance Matters More Than You Think
- How Glass Material Affects Optical Testing Results
- Core Differences Between Industrial Glass and Laboratory Glas
- How Glass Tube Ovality Affects Sealing Performance
- Why Does Sight Glass Require Independent Pressure Testing?
- How Different Annealing Processes Affect Glass Performance
- Is the Safety Valve of a Liquid Nitrogen Tank Really “Just
- Is the Safety of Tempered Glass Overestimated?